Cast Al-Si-Cu-Mg-Ni-Cr Alloy

Two-stage solution treatment

By optimizing two-stage solution and ageing treatments, the alloy achieves refined and rounded primary and eutectic silicon phases while retaining stable heat-resistant phases, significantly enhancing high-temperature mechanical properties.

Xiao, Lairong · Liu, Guanchun · Peng, Zhenwu · Tu, Xiaoxuan · Su, Heng · Xiao, Yuxiang · Zhong, Qi · Wang, Sen · Cai, Zhenyang · Zhao, Xiaojun

Materials 2023

Specifications

显微硬度峰值
{'zh': '155.82', 'en': ''} HV

Advantages

Roundness of primary Si reaches 1.46 and aspect ratio of eutectic Si reaches 2.56

High-temperature tensile properties at 350 °C improved compared to as-cast alloy