Sodium Salt Agglomeration Promoter for Quartz

Promotes agglomeration at 800°C

NaCl, Na₂CO₃ induce quartz agglomeration at 800–900°C via molten phase or low-melting sodium silicates, causing bed defluidisation.

Long, Xiaofei · Li, Jianbo · Lu, Xiaofeng · Zhang, Kai · Zhang, Dongke

Powder Technology 2023

Specifications

salt SiO ratio
{'zh': '<1.32', 'en': '<1.32'} %
for agglomeration initiation
{'zh': '155', 'en': '155'} μm
salt release rate
{'zh': '', 'en': '0.332'} min⁻¹

Advantages

Defluidisation temperature: 800–900 °C