Fine Pearlitic Steel Wire

6.5× SCC Resistance

By increasing carbon and silicon content, the pearlite lamellar spacing is refined, reducing both corrosion activity and reversible hydrogen trapping while maintaining the same tensile strength, markedly extending the time to stress corrosion fracture.

Zhang, Zeling · Qiao, Wenwei · Yan, Xu · Wang, Linfeng · Yao, Ju · Zhou, Lichu · Zhou, Xuefeng · Dargusch, Matthew Simon · Atrens, Andrej · Venezuela, Jeffrey Jones D. · Xie, Zonghan · Fang, Feng

Corrosion Science 2025

Specifications

珠光体片层间距从
{'zh': '81', 'en': ''} nm
腐蚀电流密度从
{'zh': '4.57×10⁻⁴', 'en': ''} A·cm²
可逆氢陷阱比例从
{'zh': '92.9', 'en': ''} %

Advantages

Stress corrosion fracture time extended from 8.8 h to 66.4 h