Continuous-Discontinuous Glass-Fiber Polyamide Composite

Warpage <0.1 mm, Bending Strength 400 MPa

Insert-injection moulding directly bonds continuous and short glass-fiber polyamide, providing an integrated manufacturing route for structural parts with balanced dimensional stability and mechanical strength.

Wang, Jian · Hang, Li · Fuhai, Li · Chunfeng, Fan · Liu, Tao · Da, Wang

Composites Part A: Applied Science and Manufacturing 2025

Specifications

翘曲变形低于
{'zh': '0.1', 'en': ''} mm
弯曲强度
{'zh': '400', 'en': ''} MPa
弯曲模量
{'zh': '10', 'en': ''} GPa

Advantages

Post-thermal treatment further improves mechanical properties but increases warpage