Internal curing with superabsorbent polymer significantly reduces early-age autogenous shrinkage and improves crack resistance in arid, large-temperature-variation environments.
Guo, Jinjun · Wang, Kun · Peng, Zhang · Xu, Hongyin
Construction and Building Materials 2023
28-d compressive strength increased
autogenous shrinkage reduced
crack resistance improved