Ultrasonic-Assisted Al Alloy Joint

Bonded at Low Temp, Serves High Temp

Ultrasonic vibration with an Sn-9Zn interlayer bonds Al alloy at 300°C, achieving a joint strength coefficient of 89.9% that withstands higher service temperatures.

Pu, Zhao · Li, Zhengwei · Xia, Yuanhang · Xu, Zhiwu · Leng, Xuesong · Yan, Jiuchun

Materials and Design 2023

Specifications

接头强度系数
{'zh': '89.9', 'en': ''} %

Advantages

Diffusion bonding of Al alloy at 300 °C

Sn-embedded ceramic-shell structure interface

Lowest bonding temperature among current diffusion bonding processes for Al alloys