Gradient composite amorphous filler metal

Joint shear strength 344 MPa

By adding V to the second layer of filler metal, the interfacial reaction is regulated, brittle phases are suppressed, and a joint toughened by plastic phases is obtained in K4169/TiAl joints.

Zhang, Liangliang · Li, Peng · Li, Shuai · Nie, Fuheng · Wu, Baosheng · Li, Chao · Li, Jiachen · Zhenyang, Zhang · Xin, Jiang · Bomin, Zhao · Dong, Honggang

Composites Part B: Engineering 2024

Specifications

钎焊接头剪切强度
{'zh': '344', 'en': ''} MPa
亚结构晶粒占比从
{'zh': '46.6', 'en': ''} %
高角晶界比例升
{'zh': '84.7', 'en': ''} %