Phenylalanine Electrolyte Additive

Zn anode cycle life 5250 h

An amphipathic biomolecule additives in situ constructs a nucleophilic–hydrophobic protective interphase on the Zn anode, optimizing solvation and suppressing parasitic reactions for highly reversible aqueous zinc batteries.

Anbin, Zhou · Wang, Huirong · Zhang, Fengling · Hu, Xin · Zhihang, Song · Yi, Chen · Huang, Yongxing Xin · Cui, Yanhua · Cui, Yixiu · Li, Li · Wu, Feng · Chen, Renjie

Nano-Micro Letters 2024

Specifications

全电池
{'zh': '300', 'en': ''} 次

Advantages

Zn||Zn symmetric cell cycle life up to 5250 h