Cu-Mn-Fe Prussian Blue Cathode

73.3% over 1000 cycles

Synergistic ternary composition suppresses Jahn-Teller distortion, delivering high capacity and long cycling across a wide temperature range.

Gao, Yun · Zhang, Hang · Peng, Jian · Wang, Jinsong · Liu, Xiaohao · Lingling, Zhang · Xiao, Yao · Li, Li · Liu, Yang · Qiao, Yun · Chou, Shulei

Advanced Materials 2025

Specifications

比容量
{'zh': '132.4', 'en': ''} mAh g⁻¹
次循环后容量保持率
{'zh': '73.3', 'en': ''} %
圆柱电芯
{'zh': '850', 'en': ''} 次

Advantages

Stable cycling from −20 to 55 °C