Corrosion-Resistant Li Interface
A fluorinated inorganic interphase formed via Ni2+ crossover under electron delocalization protects the Li metal anode from solvent corrosion and enables smooth deposition over long-term cycling.
Ma, Chengwei · Hongxing, Wang · Jianwei, Wang · Song, Tinglu · Zhou, Jiangqi · Li, Chunli · Xiong, Shizhao
Journal of Energy Chemistry 2025
Li metal anode surface shows smooth and flat deposition morphology after long-term cycling